Stringing and wisps

By Tony Tate · updated 2026-11-27 · First Layer 1.0.2

Most often it is one of these: wet filament, or nozzle temperature too high. Dry the spool before changing a single setting. The full list below is ordered by how often each cause is actually to blame, so work down it rather than picking the interesting one.

Fine strands spanning gaps between separate features or parts.

hairs between partscobwebsspider webs

Causes, most likely first

Ordered by how often each is actually responsible, not by how interesting it is. Work down the list.

Wet filament

Dry the spool before changing a single setting. On PETG and nylon this is often the cause, and tuning retraction on wet filament tunes around a problem you could have removed.

Nozzle temperature too high

Run a temperature tower. Over-hot plastic runs out of the nozzle on its own.

Calibration step: Run a temperature tower →

Retraction distance too short

Tune retraction distance ONLY, holding speed fixed. Changing both at once tells you nothing.

Calibration step: Tune retraction DISTANCE (only) →

Retraction too slow

Distance gets the blame and speed is half the job: retract too slowly and the nozzle is still oozing while the head leaves. Tune it on its own, after distance is settled — changing both at once tells you nothing about either.

Calibration step: Tune retraction SPEED (only) →

Travel moves too slow

Raise travel speed. Less time in the air means less time to droop a string.

Common questions

What causes stringing and wisps in 3D printing?

Wet filament. Dry the spool before changing a single setting. On PETG and nylon this is often the cause, and tuning retraction on wet filament tunes around a problem you could have removed.

What else causes stringing and wisps?

Nozzle temperature too high. Run a temperature tower. Over-hot plastic runs out of the nozzle on its own.

How do I know if it is fixed?

Change one thing at a time and reprint the same test. Fine strands spanning gaps between separate features or parts. If that is gone, the change you made was the cause; if it is not, undo it before trying the next one.

Open First Layer →
The app walks this in order, generates the test model for your nozzle and filament, and records what you measure so nothing has to be repeated. Free, no account, works offline.