ABS print settings

By Tony Tate · updated 2026-11-27 · First Layer 1.0.2

ABS prints at about 250 °C with a 100 °C bed and 0% part cooling. Usable range 235–265 °C nozzle, 90–115 °C bed. Needs an enclosure.

Acrylonitrile Butadiene Styrene

Starting settings

starting points Every number here is drawn from manufacturer data sheets across the material as a whole. None of it is a measurement of the spool in your hand, and brand-to-brand variation inside one material is wider than most people expect. Where a figure says "about", the app holds one typical value rather than a range. Treat all of it as somewhere to begin, then measure — shrinkage and flow especially, because those two are what throw dimensions off.

Nozzle
235–265 °C (start 250)
Bed
90–115 °C (start 100)
Part fan
0–25% (start 0%)
Wall speed
30–50 mm/s
Max volumetric flow
about 10 mm³/s
Shrinkage
about 0.8%
Softens at
about 105 °C
Enclosure
Required
Nozzle size
0.4 mm or larger — 0.4 mm recommended
Nozzle material
Brass is fine
Drying
about 70 °C for 4 h

Speed

Similar to PLA, 30–50 mm/s. Speed is not your constraint on this material — chamber temperature is. Slowing down does not fix warping; an enclosure does.

Bed surface

Smooth PEI at 100 °C, or glass with an ABS/acetone slurry. Wants a genuinely hot plate.

What bites people

Safety

Common questions

What temperature should I print ABS at?

Start at 250 °C nozzle and 100 °C bed, within a usable range of 235–265 °C and 90–115 °C. Run a temperature tower on your own spool rather than trusting any table: brand-to-brand variation inside one material is wider than most beginners expect.

Does ABS need an enclosure?

Yes. ABS warps and splits without one.

What nozzle do I need for ABS?

0.4 mm or larger, with 0.4 mm recommended. A brass nozzle is fine.